腻子粉厂家讲解腻子粉掉粉的原因

来源: 日期:2020-10-29 发布人:

腻子粉是建筑装饰材料的一种,主要成分是滑石粉和胶水。 刚刚购置的毛坯房表面的一层白色是腻子,通常腻子的白度在90以上细度在330以上。

Putty powder is a kind of building decoration materials, the main components are talcum powder and glue. A layer of white putty on the surface of the blank room just purchased is putty. Generally, the whiteness of putty is above 90 and the fineness is above 330.
许多腻子粉使用者不得不承认,腻子胶粉脱粉是一个很严重的问题,它会引起乳胶漆的脱落,以及腻子层的起鼓,裂缝,进而引起乳胶漆饰面发生裂缝。
Many users of putty powder have to admit that it is a very serious problem to remove the powder from the putty powder, which will cause the latex paint to fall off, and the putty layer to bulge and crack, and then cause the emulsion paint surface to crack.
腻子粉脱粉掉粉、掉白是目前常见的腻子施工后问题,要了解腻子粉脱粉的原因,首先要了解腻子粉的基本原材料组分与固化原理,然后结合腻子施工时的墙面干燥程度、吸水率,温度、天气干燥程度等。今天腻子粉厂家小编谈一谈腻子粉掉粉的主要原因,一起来看看吧!
It is a common problem after the putty construction that the putty powder degrades and whitens. To understand the reasons of the putty powder removing powder, we should first understand the basic raw material composition and curing principle of the putty powder, and then combine the dryness degree of the wall surface, water absorption rate, temperature and weather dryness degree during the putty construction. Today's putty powder manufacturers to talk about the putty powder powder off the main reason, let's have a look!

济南腻子粉
原因一
Reason one
腻子的粘结强度不够造成脱粉,生产厂家一味的降低成本,胶粉的粘结强度差,添加量较小,特别是内墙腻子,粘结强度的大小,脱粉不脱粉和胶粉以及胶水的质量和添加量有很大关系。
The adhesive strength of putty is not enough, which leads to powder shedding. The manufacturers blindly reduce the cost. The adhesive strength of rubber powder is poor, and the addition amount is small, especially for the putty of interior wall. The size of bonding strength and the quality and amount of glue powder and glue have a great relationship.
原因二
Reason two
设计配方不合理,选材的问题和结构的问题,在腻子配方中很重要。比如羟丙基甲基纤维素(HPMC)做内墙不防水的腻子,HPMC虽然很贵,但对双飞粉,滑石粉,硅灰石粉等填充料不起作用,如果仅使用HPMC就会引起脱粉,而价格低的CMC、CMS反到不脱粉,但是CMC、CMS不能做防水腻子,也不能做外墙腻子,因为CMC和CMS遇到灰钙粉、白水泥起反应,这都会引起脱粉,也有把聚丙烯酰胺加入灰钙粉、白水泥做为防水涂料,也会起化学反应引起脱粉。
Unreasonable design formula, material selection and structure are very important in putty formula. For example, hydroxypropyl methylcellulose (HPMC) is not waterproof putty for interior walls. Although HPMC is very expensive, it does not work on fillers such as Shuangfei powder, talcum powder and wollastonite powder. If only HPMC is used, it will cause de dusting. However, CMC and CMS can not be used as waterproof putty or exterior wall putty, because CMC and CMS encounter lime calcium powder and white cement Reaction, which will lead to de powdering, but also add polyacrylamide to lime calcium powder, white cement as waterproof coating, will also cause chemical reaction.
原因三
Reason 3
混合搅拌不均匀,是造成内外墙腻子脱粉的主要原因,全国有的生产厂家生产腻子粉设备简单,五花八门,不是专用搅拌设备,搅拌不均匀,引起腻子脱粉。
The uneven mixing and mixing is the main reason for the putty powder removing from the internal and external walls. Some manufacturers in China have simple and varied equipment for producing putty powder, which is not a special mixing equipment, and the mixing is uneven, which causes the putty to be powdered.
腻子粉厂家
Putty powder manufacturer
原因四
Reason four
生产工艺的错误造成腻子脱粉,如果混合搅拌机没有清扫的功能,残留较多,普通腻子中的CMC就会和防水腻子中的灰钙粉起反应,内墙腻子中的CMC、CMS和外墙腻子的白水泥起反应而造成脱粉。有的公司专用设备设置了清扫口,可以把机器中的残留物清扫干净,不仅保证腻子的质量,还可以一机多用,买一台设备生产多种腻子。
If the mixing mixer does not have the function of cleaning and there is a lot of residue, the CMC in the ordinary putty will react with the lime calcium powder in the waterproof putty, and the CMC and CMS in the inner wall putty will react with the white cement of the exterior wall putty to cause the powder removal. Some company's special equipment is equipped with cleaning mouth, which can clean up the residue in the machine, not only to ensure the quality of putty, but also to use one machine for multiple purposes. Buy one equipment to produce a variety of putty.
原因五
Reason 5
填充料的质量的不同也容易造成脱粉,内外墙腻子大量的使用填充料,但各地重钙粉、滑石粉里面Ca2CO3的含量不同,酸碱度不同也会造成腻子的脱粉,比如重庆和成都的内墙腻子粉用同样的胶粉,但滑石粉、重钙粉不同,在重庆不脱粉,在成都就脱粉,在河南、东北不脱粉,而在一些地区就脱粉。
The quality of the filler is also easy to cause the powder removal. A large number of fillers are used for the putty of internal and external walls. However, the content of ca2co3 in the putty powder of the heavy calcium powder and talc powder in different places and the pH value are different. For example, the same rubber powder is used for the interior wall putty powder of Chongqing and Chengdu, but the talcum powder and the heavy calcium powder are different. They are not powdered in Chongqing, but they are removed in Chengdu, and in Henan and East China In the north, it is not powdered, but in some areas.
原因六
Reason six
夏季外墙腻子的保水不够,特别是在大楼高层门口、窗口等高温通风的地方,灰钙粉和水泥的初凝时间不够就已失去水份,又没有养护好,也会严重脱粉。
In summer, the water retention of putty for exterior wall is not enough, especially in the high-rise building doors, windows and other places with high temperature and ventilation. If the initial setting time of lime calcium powder and cement is not enough, the moisture will be lost, and the powder will be seriously desorbed if it is not maintained well.