灌浆料的应用领域可谓多种多样,设备基础,结构加固,钢结构柱脚,预制构件,装配式建筑,水利电力风力等等,除了产品自身因素,施工不当是很容易导致高强无收缩灌浆料的使用出现问题,如何快速找到出现问题的环节,并快速解决,节省整个工期时间呢。下面是济南腻子粉厂家为您讲解过的灌浆料施工中的常见问题汇总。
The application fields of grouting materials are various, such as equipment foundation, structural reinforcement, steel structure column base, prefabricated components, prefabricated building, water conservancy, electricity and wind power. In addition to the product itself, improper construction is likely to lead to problems in the use of high-strength non shrink grouting materials. How to quickly find the problems and solve them quickly to save the whole construction period. The following is a summary of common problems in grouting material construction that Jinan putty powder manufacturer has explained to you.
01
01
缺棱掉角
Missing edges and corners
(1)模板设计未考虑防止拆模掉角因素;
(1) The template design did not consider the factor of preventing the removal of formwork from falling corners;
(2)木模未提前湿润,浇注后木模膨胀造成高强无收缩灌浆料角拉裂;
(2) The wooden mold was not moistened in advance, and the expansion of the mold after pouring caused the high-strength non-shrinkage grouting material corner to crack;
(3)模板缝不严,漏浆;
(3) Loose formwork joints and grout leakage;
(4)模板未涂刷隔离剂或涂刷不佳,造成拆模粘连;
(4) The template is not coated with isolation agent or poorly coated, resulting in adhesion during mold removal;
(5)拆模过早过猛,拆模方法及程序不当;
(5) Premature and excessive demolding, improper demolding methods and procedures;
(6)养护不好。
(6) Poor maintenance.
02
02
洞口变形
Deformation of the opening
(1)模内顶撑间太大,断面太小;
(1) The top support space inside the mold is too large and the cross-section is too small;
(2)模内无斜顶撑,刚度不足,不能保持方正;
(2) There is no diagonal support inside the mold, and the stiffness is insufficient to maintain squareness;
(3)高强无收缩灌浆料不对称浇注将模挤偏;
(3) Asymmetric pouring of high-strength non shrinkage grouting material will cause the mold to deviate;
(4)洞口模板与主体模板固定不好,造成相对移动。
(4) The fixing of the opening template and the main template is not good, causing relative movement.
济南腻子粉
03
03
错台
Wrong platform
(1)放线误差过大;
(1) Excessive setting out error;
(2)模板位移变形,支模时无须直找正措施;
(2) The displacement and deformation of the formwork do not require direct alignment measures during formwork support;
(3)下层模板顶部倾斜或涨模,上层模板纠正复位形成错台;
(3) The top of the lower formwork is tilted or expanded, and the upper formwork is corrected and reset to form a wrong platform;
04
04
板缝高强无收缩灌浆料浇筑不实
Inadequate pouring of high-strength non-shrinkage grouting material for plate joints
(1)板缝太小,石子过大;放线误差过大;
(1) The seam of the board is too small, and the stones are too large; Excessive setting out error;
(2)缝模板支吊不牢、变形、漏浆;
(2) Inadequate support, deformation, and leakage of joint formwork;
(3)缝内杂物未清,或缝内布管;
(3) Unclear debris inside the seam, or laying pipes inside the seam;
(4)无小振动棒插捣或不振捣或振捣不好。
(4) No small vibrating rod inserted or not vibrated or poorly vibrated.
灌浆料施工出现的问题在这里就从这四个方面来讲解了,希望能够给您帮助,您有什么疑惑或者需求,就来我们网站留言了解吧!